变形、挠曲、开裂
原因:采用湿铺法施工、没有预留缝隙或铺贴后未固化就上人。
预防:铺贴时用人造石专用胶黏剂,并且板与板之间留1.5~2 毫米的缝隙;铺贴 72 小时后方可行人。
起鼓(鼓包)
原因:用传统水泥砂浆铺贴人造石或粘结剂质量不佳、
预防:人造石铺贴时,基面应保证干爽,应采用专用胶黏剂而非水
泥砂浆铺贴,胶黏剂选择可靠品牌。
发黄、出现黄斑
原因:养护时使用钢丝棉上光,但钢丝棉生锈,铁锈粉污染石材板面,出现发黄现象;使用了石蜡进行养护。
预防:选用不锈钢材质的钢丝棉上光;选用渗透性养护剂。
Construction FAQs
Deformation, deflection, cracking
Reason: The use of wet paving method construction, no gaps are reserved or paved without curing.
Prevention: Use a special adhesive for artificial stone when paving, and leave a gap of 1.5 to 2 mm between the boards; paving for 72 hours before pedestrians.
Drumming (Drum Pack)
Cause: Poor quality of paving artificial stone or binder with traditional cement mortar,
Prevention: When laying artificial stone, the base surface should be kept dry, and special adhesives should be used instead of water
Mud mortar paving, adhesive selection reliable brand.
Yellowing, macula
Reason: Steel wool is used for maintenance, but steel wool rusts, rust powder pollutes the stone plate surface, and yellowing occurs; paraffin wax is used for maintenance.